TYPE: span> |
70/100 span> |
Test Method span> |
Penetration at 25 ºC, 0,1 mm |
70-100 |
EN 1426 |
Softening method "ring and ball", º C |
43-51 |
EN 1427 |
temperature breakage Fraas, º C |
- 10 |
EN 12595 |
K inematichen in viscosity 135 º C mm2 / s, min |
230 |
EN 12595 |
Flash point, º C min |
230 |
EN ISO 2592 |
Resistance to hardening / hardening in 163 ºC |
|
|
- change in mass%, +/- max |
0.8 |
EN 12607-1 |
- preserved penetration%, min |
46 |
EN 12607-1 |
- the softening temperature by the "ring and ball" after hardening / tempering ºC, min |
45 |
EN 12607-1 |
Temperature softening method "ring and ball" increase ºC, max |
9 |
EN 1727 |
Solubility% m / m min |
99.0 |
EN 12592 |